Accelerator NL51P |
|
Cobalt octoate, phthalate solvent |
|
136-52-7 |
|
Cobalt(II) 2-ethylhezanoate, 6% Co, in aliphatic ester. The curing of unsaturated polyester resins at ambient temperatures can in general not be performed by an organic peroxide alone. The radical formation, which i snecessary to start the polymerization reaction, is at ambient temperatures with most generally applied organic peroxides too slow. To speed up the radical formation in a controllable way organic peroxides must therefore be used in combination with a so-called accelerator. |
|
Balance: 40% TXIB, 25% mainly white spirit TSCA: registered Appearance: clear blue violet liquid Cobalt content: 6.0 +/- 0.1% Density,20'C: 963 kg/m3 Viscosity,20'C: 16 mPa.s Flashpoint: 72'C (Abel-Pensky,CC) Sulubility : insoluble in water. Soluble in various organic solvents. |
Industrial field |
plastic, polymer, resin, monomer |
|
|
|
|
|
|
|