Accelerator 55028 |
|
Cobalt octoate, hydrocarbon solvent |
|
136-52-7 |
|
Mixture of cobalt(II) 2-ethylhexanoate and barium carboxylate, 2.25% co, in solvents. The curing of unsaturated polyester resins at ambient temperatures can in general not be performed by an organic peroxide alone. The radical formation, which is necessary to start the polymerization reaction, is at ambient temperatures with most generally applied organic peroxides too slow. To speed up the radical formation in a controllable way organic peroxides must therefore be usde in combination with a so-called accelerator. |
|
Balance: 50% Organic solvents, mainly white spirit TSCA: registered Appearance: clear blue violet liquid Cobalt content: 2.25 +/- 0.05% Density,20'C: 940 - 960 kg/m3 Flashpoint: 39'C(Cleveland,OC) Solubility : Insoluble in water. Soluble in various organic solvents. |
Industrial field |
additive, plastic, polymer, resin, monomer |
|
|
|
|
|
|
|
There are no existing companies to distribute selected chemical product |
|
|
|
|
|