Aflas FA 100H |
|
Di-polymer of tetrafluoroethylene and propylene |
|
Aflas FA 100H can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical TFE elastomer formulations. The "dry"ingredients should be blended before adding to the masticated gum. For best results, FA 100H should be banded on the mill several minutes prior to adding the blended dry ingredients. For internally mixed compounds, a two-pass procedure is recommended, with the peroxide being added in the second pass. Once mixed, the compounded stocks have good scorch resistance and storage stability. |
|
Fluorine Content [3M 36.4]: 57.0% Specific Gravity [ASTM D297]: 1.55 Color: Dark Brown Solubility: Freon TF or Tetrahydrofuran |
|
|
|
|
|
|
|