ESCORENE ULTRA LD 783 |
|
Ethylene Vinyl Acetate Copolymer |
|
24937-78-8 |
|
Escorene Ultra LD 783 is a 33 wt% vinyl acetate copolymer. * Applications: -Soft, injection molded parts -Low modulus applications |
|
Melt Index (g/10 min): 43 Vinyl Acetate (wt%): 33 Density (g/cm): 0.956 Peak Melting Temperature 'F('C): 142(61) Bulk Density lb/ft(kg/m): 36(577) Softening Point, R & B 'F('C): 221(105) Tensile Strength @ Break psi (MPa): 440(3.0) Elongation @ Break (%): 1050 |
|
|
|
|
|
|
|